Storage conditions of plastic pellets
Temperature 23 ± 2, humidity 50 ± 5. When organic matters contact with air, they will oxidize slowly and heat will be released during the oxidation process. When the plastic particles are piled up, the internal ventilation is not good, and the thermal conductivity of the plastic is poor, the heat generated by oxidation will slowly accumulate, and with the increase of temperature, the oxidation rate will also increase, when the temperature exceeds the burning point of the plastic, it will cause spontaneous combustion. The method to prevent the spontaneous combustion of plastic is very simple. As long as the plastic particles are put into the bag, the bag is stacked neatly, and the space between the bags is used to ensure enough air circulation, so as to avoid the uncontrolled temperature rise of the plastic particles
If you want to know more about it please do not hesitate to
contact me. WhatsApp:+86-15966835076.